Both laser welding and electron beam welding (EBW) produce deep-penetration keyhole welds with narrow heat-affected zones and high aspect ratios. In the right application, each outperforms the other decisively. The choice is not primarily about weld quality — both processes can achieve equivalent weld quality on suitable materials — but…
Pipe and tube welding is one of the highest-consequence laser welding applications — fluid systems carry gases and liquids under pressure, and a weld defect that is cosmetically invisible becomes a leak path or a fracture initiation site in service. The laser welding characteristics that matter most for pipe and…
Jewelry laser welding operates at a completely different scale from industrial sheet metal welding — spot sizes of 0.1–1.0 mm, pulse energies of 1–100 joules, and weld depths of 0.1–0.8 mm — but the underlying physics are the same keyhole and conduction-mode mechanisms that govern all laser welding. What differentiates…
Sheet metal cabinet and enclosure manufacturing is one of the largest production application segments for laser welding — larger in total weld volume than the automotive or aerospace sectors combined for shops in the electrical cabinet, server rack, HVAC, and industrial control panel markets. The reasons are production-specific: cabinets are…
The consumer appliance and kitchenware manufacturing sector adopted laser welding in the 1990s and has never gone back to TIG. The reason is straightforward: TIG welding thin stainless steel produces a heat-discolored, wide-HAZ weld that requires significant post-weld grinding and polishing before any surface finish can be applied or preserved.…
Laser welding brass is technically possible but governed by a material constraint that does not appear in steel or stainless welding: zinc’s boiling point (907°C) is lower than brass’s melting point (900–940°C for the weld pool interface). Unlike galvanized steel — where the zinc coating is external and can be…
Battery manufacturing is the fastest-growing application segment for laser welding, driven by electric vehicle production and grid-scale energy storage. The specific demands of battery welding — thin dissimilar metal joints, zero tolerance for spatter contamination inside cells, electrical resistance as the primary quality metric rather than tensile strength, and production…
Burn-through in thin sheet metal laser welding is not simply “too much power” — it is a specific sequence: the keyhole penetrates the full material thickness and breaks through the root, the back-surface support for the weld pool is lost, the pool collapses, and liquid metal falls through the joint.…
Dissimilar metal laser welding is possible for some combinations, marginal for others, and not feasible by fusion welding for several commercially important pairs. The determining factor is not welding technique or process optimization — it is the metallurgy of the interface between the two metals during and after solidification. Specifically:…
Galvanized steel presents a specific welding problem that has nothing to do with the steel itself: the zinc coating boils at 907°C, while steel melts at approximately 1,500°C. By the time the laser has heated the steel substrate to its melting point, the zinc coating has already vaporized — and…